Email Us

Issues and Technical Resolutions in Water-based Steel Drum Paint

  1. Contraction

During the painting or drying process of the paint film, the surface of the topcoat may exhibit wrinkles, shrinkage, and deformation. This particular defect is most commonly observed in alkyd paint repair operations.

Cause:

Improper drying methods result in uneven drying of the paint surface. If the newly applied paint layer is dried too quickly or subjected to forced drying, or if the temperature within the paint shop is excessively high, the surface paint dries rapidly and contracts. This, in turn, delays the drying process of the underlying paint layer. When the inner coating eventually dries, it causes the surface coating to shrink. To avoid this, refrain from painting in workshops with unsuitable temperatures or those experiencing significant temperature fluctuations.

  1. Elevation

Elevations, also known as wrinkles, manifest as protrusions during the spraying or drying process of the paint film. These bumps can assume various shapes due to the expansion of the paint surface.

Cause:

  1. Inadequate cleaning of the underlying layer. For instance, if grease or wax on the bottom surface is not thoroughly removed, the subsequently applied paint fails to adhere properly due to the interlayer effect.

  2. Insufficient interval time between the first and second sprayings, depriving the primer of ample drying time. Consequently, the moisture present in the wet paint surface corrodes the primer or topcoat, rendering it soft.

Correction method:

Smooth out the defective area through careful polishing, ensuring not to wear through the surface, and proceed with repainting.


Popular Drum Barrel Fittings

Related Drum Accessories and Fittings News & Blog

  • What To Know After The Spring Festival (1)What To Know After The Spring Festival (1)July 4, 2022Individual protective equipment1. Safety helmet has no aging, no damage, and no artificial maintenance and transformation.2. Properly wear helmet: Hat is properly worn and the hat band is tight.3. Wea...view
  • SWIFT Code Or IBAN?SWIFT Code Or IBAN?June 30, 2022Doing international trades may come down to bank transfer, which may need your bank SWIFT Code or IBAN. The two numbers are chosen among different regions across the world. The answer is as below:IBAN...view
  • Environmental Progress of Steel Drum ClosuresEnvironmental Progress of Steel Drum ClosuresJune 10, 2023Electroplating, painting and other processes in the production process of steel drums are major causes of water pollution and air pollution. Therefore, in the cause of environmental protection, our st...view
  • Performance Characteristics of Steel DrumsPerformance Characteristics of Steel DrumsJuly 17, 2023Although the application of steel drums has only a history of more than 100 years, it has developed rapidly and has a wide variety of varieties, which are widely used in industrial product packaging, ...view
  • The Price Trend Of Construction SteelThe Price Trend Of Construction SteelJuly 1, 2022Construction steel: On April 8, the average price of 20mm three-level seismic rebar steel in 31 major cities in China was RMB5123 / ton, down by RMB5 / ton compared with the previous trading day. This...view
  • Function Of Galvanization And Its Operating PrincipleFunction Of Galvanization And Its Operating PrincipleJuly 1, 2022Function:Galvanizing the metal can make it corrosion resistant.Without protective zinc coating, metal will always be exposed to elements and will be oxidized and corroded faster.In terms of corrosion ...view
Tel
86-18768445568
Address
No.58 Qinjian Road, Hengshan Industrial Park, Shouchang Town, Jiande City, Zhejiang Province, China