The uneven appearance of the paint coating, which resembles the peel of an orange or walnut, is called orange peel.
The reasons are as follows:
1) The construction viscosity is too high and the paint film leveling is poor;
2) Improper selection of spray gun;
3) High temperature and low humidity in the spray room;
4) Insufficient leveling time and premature entry into the drying room;
5) Spraying film is too thick or too thin
Solutions:
1) Add pure water to adjust the coating viscosity;
2) Standardize the spray gun, or adjust the spraying distance, fan width, etc.;
3) Reduce the temperature of the spray room, improve the humidity of the spray room;
4) Increase leveling time;
5) Adjust the amount of spit and gun speed to prevent the paint film thickness beyond the specified range.
Short comments: in the process of painting epoxy phenolic drum closures, the orange peel probelm will also occur, but with small probability, we will check each closures for customers.
Spot Market For Raw MaterialsJuly 1, 2022Import mine: on April 8th, the spot market activity of imported iron ore in the area along the Yangtze River has picked up somewhat compared with the earlier stage, the trade newspaper has improved th...view
55 Gallon Drum: The Ideal Choice for a Multi-Purpose ContainerJune 5, 202355-gallon drum, also known as a steel drum, is a versatile container that is widely used in different fields. It is made of high-quality plastic or metal, and has the characteristics of durability, re...view
Urgent Notice! 15 Grade Typhoon CANDU About To Land, Port Closed!June 30, 2022At 06:00 on September 13, the Central Meteorological Observatory continued to issue orange typhoon warning.At 5 a.m. yesterday (13th), the center is located in the sea about 185km southeast of Xiangsh...view